With fibrillation, PBO fiber turns into pulp, which could be applied in specialty paper, friction and sealing material, as well as reinforced plastics or reinforced rubber manufacturing.
Pulp |
Unit |
|
Chemical composition |
/ |
PBO |
Cut length |
mm |
0.5-1.4 |
Specific surface area |
m2/g |
6.5-15 |
Moisture content |
% |
4 |
Oil content |
% |
0-2 |
Freeness |
ml |
200-450 |